Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering N70L Nitrile Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering N70L Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nitrile Butadiene Rubber (NBR), 70 °IRHD. Low- Med acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet: ASTM D2000/SAE J200 line call-out: M5BG710, A14, B14, EO14, EO34, F17.Applications: The low acrylonitrile content of this compound provides excellent low temperature flexibility, in sealing conditions where resistance to mineral oil, alcohol, paraffin and low-aromatic petrol is required. Not recommended for use with acetone, benzene, chlorinated solvents or high-aromatic petrol. Good water resistance but poor against ozone and weather.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
55 - 85
55 - 85
°IRHD, ±15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield >= 8.00 MPa
>= 1160 psi
-20% change after 70 hours @ 100°C; ASTM D412
>= 10.0 MPa
>= 1450 psi
ASTM D412
Elongation at Break >= 150 %
>= 150 %
-40% change after 70 hours @ 100°C; ASTM D412
>= 250 %
>= 250 %
ASTM D412
Compression Set <= 25 %
<= 25 %
22 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F
Users viewing this material also viewed the following: