3M 9832 Double Coated Tapes with Adhesive 300MP

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9832 Double Coated Tapes with Adhesive 300MP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape is well suited for applications requiring temperature performance up to 250°F for short term exposure and up to 150°F for long term exposure. A thin polyester film carrier provides dimensional stability and improved handling.Information provided by 3M
Physical Properties Metric English Comments
Thickness 12.7 microns
0.500 mil
Carrier
50.8 microns
2.00 mil
Backside Adhesive
58.4 microns
2.30 mil
Faceside Adhesive
102 microns
4.00 mil
Liner Caliper
122 microns
4.80 mil
Total Thickness
Mechanical Properties Metric English Comments
Peel Strength 0.3725 kN/m
2.125 pli
Polypropylene, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.614 kN/m
3.50 pli
Stainless Steel, 90°, 15 min RT; ASTM D3330
0.6355 kN/m
3.625 pli
Stainless Steel, 90°, 72 hr RT; ASTM D3330
0.6355 kN/m
3.625 pli
ABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.7231 kN/m
4.125 pli
Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.9422 kN/m
5.375 pli
Stainless Steel, 90°, 72 hr 158°F; ASTM D3330
1.030 kN/m
5.875 pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 65.6 °C
150 °F
Long Term
121 °C
250 °F
Short Term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Liner Tan, 58# Polycoated Kraft