Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Lo-Skid® LS7000/LS7100 Series High Density Bumper and Footpad Urethane Foam

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Lo-Skid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Lo-Skid® LS7000/LS7100 Series High Density Bumper and Footpad Urethane Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Lo-Skid™ LS7000 and LS7100 (acrylic adhesive on one side) urethane foam products are widely recommended for bumpers and footpads for applications and electronic products because it provides a high coefficient of surface friction combined with a smooth non-marring surface. Lo-Skid is flexible and can be die-cut to the required size and shape. Features/Benefits: High coefficient of friction; Abrasion resistance; Flexible and conformable; High durometer - will withstand heavy loads; Smooth, non-marring surface; Thicknesses from 16 mils to 125 mils. Typical Applications: Foot pads and bumpers for business machines, housewares, industrial equipment, electronics.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 0.637 g/cc
0.0230 lb/in³
ASTM D1667
Mechanical Properties Metric English Comments
Hardness, Shore O 65
65
ASTM D2240
Tensile Strength, Yield 3.07 MPa
445 psi
ASTM D3574
Elongation at Break 300 %
300 %
ASTM D3574
Tensile Modulus 0.00172 GPa
0.250 ksi
ASTM D3574
Compressive Strength 0.448 MPa
65.0 psi
Compression Deflection, Value given for 12.7 mm/min, 25% deflection.; ASTM D3574 Test C
Compressive Modulus 0.000758 GPa
0.110 ksi
Force to Compress, Value given for 25% compression; ASTM D1667
Coefficient of Friction, Dynamic 1.4
1.4
ASTM D4518
Tear Strength 10.5 kN/m
60.0 pli
Initial Tear Strength; ASTM D624 Die C
Compression Set <= 5.0 %
<= 5.0 %
Constant Deflection at 73°F; ASTM D 3574 Test D
<= 35 %

@Temperature 70.0 °C
<= 35 %

@Temperature 158 °F
Constant Deflection; ASTM D 3574 Test D
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
Constant use
121 °C
250 °F
Intermittent
Users viewing this material also viewed the following: