Polymer Property : Thermal Conductivity = 243 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 35.0 W/m-K

@Temperature 85.0 °C
243 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy 170 Pure Lead
Information Provided by Indium Corporation
Thermal Conductivity 35.0 W/m-K

@Temperature 85.0 °C
243 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 181 Sn-Pb-Cd Solder Alloy
Good general purpose solder in the medium temperature range. Maintains its creep strength well. Not applicable against gold.Information provided by the manufacturer, Indium Corporation.
Thermal Conductivity 35.0 - 50.0 W/m-K
243 - 347 BTU-in/hr-ft²-°F
Indium Corp. NanoFoil® High Temperature Nickel and Aluminum Sacrificial Heat Source
As a sacrificial heat source in soldering and brazing applications, NanoFoil® is ideal for high-temperature applications. NanoFoil becomes a non-functional part of the solder or braze joint, eli..
Thermal Conductivity 35.0 W/m-K
243 BTU-in/hr-ft²-°F
Materion Beryllium Nickel M220C
Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor..
Thermal Conductivity 35.0 - 50.0 W/m-K
243 - 347 BTU-in/hr-ft²-°F
Indium Corp. NanoFoil® NF40 Nickel and Aluminum Localized Heat Source For Bonding
Features:40 microns thick - optimized for bonding electronics assembliesMinimum dimension 1.2mm x 2.0mmLocalized heat source for bondingEnables high-strength, high conductivity bonds between most co..
Thermal Conductivity 35.0 W/m-K
243 BTU-in/hr-ft²-°F
Sapco Silicon Nitride, Si3N4
Information provided by Sapco.
Thermal Conductivity 35.0 W/m-K
243 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS314A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 35.0 - 40.0 W/m-K
243 - 278 BTU-in/hr-ft²-°F
Goodfellow Ruby, Al2O3
Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro..
Thermal Conductivity 35.0 W/m-K
243 BTU-in/hr-ft²-°F
California Fine Wire Nickel Alloy 180 Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Thermal Conductivity 35.0 W/m-K
243 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 147-5 Silicon Nitride
Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradyne's..
Thermal Conductivity 35.0 W/m-K
243 BTU-in/hr-ft²-°F
China-Yixing Longly Refractories 99 Alumina Ceramic
LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, ..