Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Williams Advanced Alloys WS314A Solder

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS314A Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 10.8 g/cc
0.390 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.6 MPa
4000 psi
Thermal Properties Metric English Comments
CTE, linear 28.4 µm/m-°C

@Temperature 20.0 °C
15.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 35.0 W/m-K
243 BTU-in/hr-ft²-°F
Melting Point 310 - 314 °C
590 - 597 °F
Solidus 310 °C
590 °F
Liquidus 314 °C
597 °F
Component Elements Properties Metric English Comments
Lead, Pb 95 %
95 %
Tin, Sn 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00002123 ohm-cm
0.00002123 ohm-cm
Users viewing this material also viewed the following: