Material Notes:
Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradyne's silicon nitrides. Finished components are machined at Ceradynes precision diamond grinding facility.Applications: wear components.Information provided by Ceradyne Company
Physical Properties Metric English Comments
Density 3.30 g/cc
0.119 lb/in³
Weibull Modulus 15 - 20
15 - 20
Mechanical Properties Metric English Comments
Vickers Microhardness 1800
1800
0.3
Modulus of Elasticity 320 GPa
46400 ksi
Flexural Strength 930 MPa

@Temperature 23.0 °C
135000 psi

@Temperature 73.4 °F
Poissons Ratio 0.28
0.28
Fracture Toughness 6.00 MPa-m½
5.46 ksi-in½
Shear Modulus 125 GPa
18100 ksi
calculated
Abrasion 1100
1100
Abrasive Wear Resistance Parameter
Thermal Properties Metric English Comments
CTE, linear 3.20 µm/m-°C

@Temperature 20.0 - 1000 °C
1.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 35.0 W/m-K
243 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 8.14
8.14
Descriptive Properties Value Comments
Purity, % >98.5
Thermal Shock Parameter 654°C