Thermal Properties Metric English Comments
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
McDanel Advanced Ceramics SiAlON
Information provided by McDanel Advanced Ceramic Technologies.
Thermal Conductivity 21.0 W/m-K

@Temperature 85.0 °C
146 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy 11 Lead Solder Alloy
Information Provided by Indium Corporation
Thermal Conductivity 21.0 W/m-K

@Temperature 20.0 °C
146 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel TENASTEEL® Cold Work Tool Steel
Description: TENASTEEL is a cold work tool steel, combining a high wear resistance together with a very high toughness. Its other advantages are a good machinability in the as-delivery condition and..
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
Momentive Performance Materials Zirconium Carbide (ZrC) Coating
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i..
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
DIN EN 821-2
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3
SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an..
Thermal Conductivity 21.0 W/m-K

@Temperature 20.0 - 100 °C
146 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
DIN EN 821-2 / ASTM-C408
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3
SL 200 ST is a silicon nitride ceramic especially suitable for components exposed to mechanical stress and engine-specific applications even at elevated temperatures. It is recognized for its high s..
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS314 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
California Fine Wire Nico Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
California Fine Wire Stablohm 750 Chromium, Aluminum, and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
China-Yixing Longly Refractories 95 Alumina Ceramic Tubes & Rods
LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat..
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
CeramTec 965 Toughened Alumina (Al2O3-ZrO2)
Hasselman Thermal Shock value is 270 K.Data provided by CeramTec North America.
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
CeramTec SL200B Silicon Nitride
SL200B ceramic material was designed especially for use in the field of welding technology. SL200B is a 100 bar gas-pressure sintered silicon nitride (Si3N4) with impressive properties. It boasts de..