Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy 11 Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 11 Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 11.06 g/cc
0.3996 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 6.0

@Load 100 kg,
Time 30.0 sec
6.0

@Load 220 lb,
Time 0.00833 hour
Tensile Strength at Break 29.9 MPa
4330 psi
Elongation at Break 52 %
52 %
Shear Strength 22.2 MPa
3220 psi
Thermal Properties Metric English Comments
CTE, linear 29.0 µm/m-°C

@Temperature 20.0 °C
16.1 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 21.0 W/m-K

@Temperature 85.0 °C
146 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 300 - 313 °C
572 - 595 °F
Solidus 300 °C
572 °F
Liquidus 313 °C
595 °F
Component Elements Properties Metric English Comments
Indium, In 5.0 %
5.0 %
Lead, Pb 95 %
95 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000340 ohm-cm
0.0000340 ohm-cm