Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials Zirconium Carbide (ZrC) Coating

Category Ceramic , Carbide , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Momentive Performance Materials (Former GE Advanced Ceramics)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Zirconium Carbide (ZrC) Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance in the sealing and protecting of graphite hardware from hot ammonia, hydrogen, hydrochloric acid, and molten metals used in compound semiconductor epitaxial processes such as MOCVD and LPE. These carbide coatings are uniform, impermeable, electrically conductive, and extremely wear resistant thus providing long life and low particle generation.Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.
Physical Properties Metric English Comments
Density 6.70 g/cc
0.242 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 350 - 400 GPa
50800 - 58000 ksi
Young's modulus
Compressive Strength 820 MPa
119000 psi
Thermal Properties Metric English Comments
CTE, linear 6.70 µm/m-°C

@Temperature 20.0 °C
3.72 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
Melting Point 3540 °C
6400 °F
Maximum Service Temperature, Air 800 °C
1470 °F
oxidation limit
Optical Properties Metric English Comments
Emissivity (0-1) 0.40
0.40
normal spectrum
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000500 ohm-cm
0.0000500 ohm-cm
Users viewing this material also viewed the following: