Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 11.06 g/cc
0.3996 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 29.9 MPa
4330 psi
Thermal Properties Metric English Comments
CTE, linear 29.0 µm/m-°C

@Temperature 20.0 °C
16.1 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
Melting Point 300 - 314 °C
572 - 597 °F
Solidus 300 °C
572 °F
Liquidus 314 °C
597 °F
Component Elements Properties Metric English Comments
Indium, In 5.0 %
5.0 %
Lead, Pb 95 %
95 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00003372 ohm-cm
0.00003372 ohm-cm
Users viewing this material also viewed the following: