Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 1390 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 50.0 - 200 W/m-K
347 - 1390 BTU-in/hr-ft²-°F
NanoAmor 50% Regular Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an..
Thermal Conductivity 50.0 - 200 W/m-K
347 - 1390 BTU-in/hr-ft²-°F
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Thermal Conductivity 195 - 200 W/m-K
1350 - 1390 BTU-in/hr-ft²-°F
x-y direction
MarkeTech Cu/Mo/Cu 1:5:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
Thermal Conductivity 190 - 200 W/m-K
1320 - 1390 BTU-in/hr-ft²-°F
x-y direction
MarkeTech Cu/Mo/Cu 13:74:13 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
Thermal Conductivity 190 - 200 W/m-K
1320 - 1390 BTU-in/hr-ft²-°F
MarkeTech Mo70Cu Moly/Copper Heat Sink Material
MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivit..
Thermal Conductivity 190 - 200 W/m-K
1320 - 1390 BTU-in/hr-ft²-°F
MarkeTech W85Cu Tungsten/Copper Heat Sink Material
WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c..
Thermal Conductivity 190 - 200 W/m-K
1320 - 1390 BTU-in/hr-ft²-°F
MarkeTech WCu15 Tungsten Copper Alloy
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Thermal Conductivity 130 - 200 W/m-K
902 - 1390 BTU-in/hr-ft²-°F
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Thermal Conductivity 10.0 - 200 W/m-K
69.4 - 1390 BTU-in/hr-ft²-°F
Alliance A-5S Alnico Magnetic Material
Thermal Conductivity 10.0 - 200 W/m-K
69.4 - 1390 BTU-in/hr-ft²-°F
Alliance A-8S Alnico Magnetic Material
Thermal Conductivity 160 - 200 W/m-K
1110 - 1390 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 1370CS AlN
Applications:replacement for 99.5 BeOcollector rodshelix supportswindowsFeatures: higher thermal conductivity than BeO at high temperatures.Information provided by Ceradyne Company
Thermal Conductivity 10.0 - 200 W/m-K
69.4 - 1390 BTU-in/hr-ft²-°F
Alliance A-6S Alnico Magnetic Material
Thermal Conductivity 10.0 - 200 W/m-K
69.4 - 1390 BTU-in/hr-ft²-°F
Alliance A-2S Alnico Magnetic Material