Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 902 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Poco Graphite AXF-5Q10W Biomedical Grade Graphite
POCO has developed post synthesis modifications to make our graphites more suitable to specific conditions. As a producer of highly technical, specialty materials, POCO also offers design engineerin..
Thermal Conductivity 130 - 200 W/m-K
902 - 1390 BTU-in/hr-ft²-°F
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Superior Die Set FORTAL® HR Aluminum Alloy
Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and d..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
UCAR Carbon UCAR® PGW Pressure Molded Graphite
An economical low ash material with excellent thermal shock resistance, Grade PGW is well suited for the fine machining detail required in molds for casting metal shapes. Grade PGW is a molded versi..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
TIMCAL TIMREX® T150 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
TIMCAL TIMREX® T15-75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
TIMCAL TIMREX® T200-2000 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
powders pressed to density of 2.2 g/cm<sup>3</sup>
TIMCAL TIMREX® T75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
TIMCAL TIMREX® T800 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
TIMCAL TIMREX® T150-600 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Temper T851
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..
Thermal Conductivity 130 - 140 W/m-K
902 - 972 BTU-in/hr-ft²-°F
Constellium PLAN 5754 Aluminum Rolled Plate
Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m..
Thermal Conductivity 130 - 140 W/m-K
902 - 972 BTU-in/hr-ft²-°F
Constellium PLAN OX 5754 Aluminum Rolled Plate
Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
CMW® 73 Copper Alloy
CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Aleris Weldural Aluminum Alloy, 400 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Aleris Weldural Aluminum Alloy, 600 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Aleris Weldural Aluminum Alloy, 100 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Aleris Weldural Aluminum Alloy, 200 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Aleris Weldural Aluminum Alloy, 300 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Aleris Weldural Aluminum Alloy, 500 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Aleris Weldural Aluminum Alloy, 700 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 2710 BeO-SiC
Applications:terminationssever wedgesload pelletsabsorbersFeatures: former industry standard for terminations etc.Information provided by Ceradyne Company
Copyright © lookpolymers.com All Rights Reserved