Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NanoAmor 50% Regular Single Walled Carbon Nanotubes

Category Carbon
Manufacturer Nanostructured & Amorphous Materials Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoAmor 50% Regular Single Walled Carbon Nanotubes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption and shieldingEnergy conversionLithium-battery anodesHydrogen storageNanotube composites (by filling or coating)Nanoprobes for STM, AFM, and EFM tips, nanolithography, nanoelectrodes, drug delivery, sensorsReinforcements in compositesSupercapacitorInformation provided by NanoAmor Inc.
Physical Properties Metric English Comments
Particle Size 0.0011 µm
0.0011 µm
Average, from Raman Spectra
0.00080 - 0.0016 µm
0.00080 - 0.0016 µm
from Raman Spectra
0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
from HRTEM
Specific Surface Area >= 400 m²/g
>= 400 m²/g
Mechanical Properties Metric English Comments
Modulus of Elasticity 10.0 - 1000 GPa
1450 - 145000 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 50.0 - 200 W/m-K
347 - 1390 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0100 - 10000 ohm-cm
0.0100 - 10000 ohm-cm
Descriptive Properties Value Comments
Color black
Length (um) 5-15
Purity (vol% carbon nanotubes), min 90
Purity (vol% single-walled nanotubes), min 50
Users viewing this material also viewed the following: