MarkeTech Mo70Cu Moly/Copper Heat Sink Material

Category Metal , Metal Matrix Composite , Nonferrous Metal , Molybdenum Alloy , Refractory Metal
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Mo70Cu Moly/Copper Heat Sink Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivity. Other features includeSheets can be stamped when moly is less than 70%Non magneticCan be gold or nickel platedData provided by the supplier, MarkeTech International.
Physical Properties Metric English Comments
Density 9.60 - 9.80 g/cc
0.347 - 0.354 lb/in³
Thermal Properties Metric English Comments
CTE, linear 7.80 - 8.40 µm/m-°C

@Temperature 20.0 - 100 °C
4.33 - 4.67 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 190 - 200 W/m-K
1320 - 1390 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 30 %
30 %
Molybdenum, Mo >= 70 %
>= 70 %