Thermal Properties Metric English Comments
Thermal Conductivity 100 - 130 W/m-K
694 - 902 BTU-in/hr-ft²-°F
MarkeTech AN 120 Aluminum Nitride Ceramic Substrate, 98% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
Thermal Conductivity 100 W/m-K
696 BTU-in/hr-ft²-°F
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 100 W/m-K
696 BTU-in/hr-ft²-°F
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 100 W/m-K
696 BTU-in/hr-ft²-°F
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 100 W/m-K
696 BTU-in/hr-ft²-°F
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 100 W/m-K
696 BTU-in/hr-ft²-°F
Materion BrushCAST® 165CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Thermal Conductivity 100 W/m-K
696 BTU-in/hr-ft²-°F
Materion BrushCAST® 165C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
Sapco S.SiC Silicon Carbide
Information provided by Sapco.
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
UCAR Carbon UCAR® ATR Isostatic Molded Graphite
Isostatically molded ATR is a lower density version of grade ATJ. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish.Typical Application..
Thermal Conductivity 100 W/m-K

@Temperature 20.0 - 100 °C
694 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
DIN EN 821-2
CeramTec CD 101 Silicon Carbide, SiC-ZrB2
CD101 is a zirconia reinforced silicon carbide designed for maximum hardness.
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
DIN EN 821-2
CeramTec CD 110 Silicon Carbide, SSiC
Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applicati..
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
DIN EN 821-2
CeramTec Rocar® ST Silicon Carbide, SSiC
Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat..
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
CoorsTek ACI-Co6 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
ASTM C408
CoorsTek SC-BNL (SC-42) Loaded Reaction Bonded Silicon Carbide
Thermal Shock Delta Tc = 137°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
ASTM C408
CoorsTek Tungsten Carbide, WC
Information provided by CoorsTek.
Copyright © lookpolymers.com All Rights Reserved