Sapco S.SiC Silicon Carbide

Category Ceramic , Carbide
Manufacturer Sapco
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sapco S.SiC Silicon Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sapco.
Physical Properties Metric English Comments
Density 3.10 g/cc
0.112 lb/in³
Open Porosity 0.00 %
0.00 %
Weibull Modulus 10
10
Mechanical Properties Metric English Comments
Hardness, Mohs 9.0
9.0
Tensile Strength, Ultimate 450 MPa
65300 psi
Modulus of Elasticity 410 GPa
59500 ksi
Flexural Strength 410 MPa
59500 psi
Compressive Strength 2000 MPa
290000 psi
Poissons Ratio 0.17
0.17
Shear Modulus 175 GPa
25400 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 3.80 µm/m-°C

@Temperature 20.0 °C
2.11 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.00 J/g-°C
0.239 BTU/lb-°F
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1400 °C
2550 °F