Material Notes:
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
Physical Properties Metric English Comments
Density 14.9 g/cc
0.538 lb/in³
Particle Size 1.0 - 3.0 µm
1.0 - 3.0 µm
Grain Size
Mechanical Properties Metric English Comments
Hardness, Rockwell A 92
92
Modulus of Elasticity 627 GPa
90900 ksi
Flexural Strength 1930 MPa
280000 psi
Poissons Ratio 0.21
0.21
Shear Modulus 259 GPa
37600 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 4.70 µm/m-°C

@Temperature 25.0 - 400 °C
2.61 µin/in-°F

@Temperature 77.0 - 752 °F
5.30 µm/m-°C

@Temperature 25.0 - 800 °C
2.94 µin/in-°F

@Temperature 77.0 - 1470 °F
Specific Heat Capacity 0.2093 J/g-°C
0.05002 BTU/lb-°F
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F