Material Notes:
Polyethylene terephthalate film is a flexible film with high mechanical resistance. An excellent insulator, it preserves all its properties in a wide range of temperatures (-70°C to +150°C). Available in a range of thicknesses from 1.5 µm to 480 µm. Excellent resistance to most chemical agents. Theoretically impermeable to nearly all reagents, solvents and lacquers.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 1.395 g/cc
1.395 g/cc
Water Absorption <= 0.80 %
<= 0.80 %
ASTM D3418-82
Thickness 19.0 - 23.0 microns
0.748 - 0.906 mil
Mechanical Properties Metric English Comments
Tensile Strength 190 - 200 MPa
27600 - 29000 psi
ASTM D882-80
Elongation at Break 130 - 190 %
130 - 190 %
ASTM D882-80
Thermal Properties Metric English Comments
Thermal Conductivity 0.150 W/m-K
1.04 BTU-in/hr-ft²-°F
Melting Point 250 - 258 °C
482 - 496 °F
Shrinkage 3.5 - 4.5 %

@Temperature 200 °C,
Time 1800 sec
3.5 - 4.5 %

@Temperature 392 °F,
Time 0.500 hour
ASTM D1204-78
Electrical Properties Metric English Comments
Dielectric Constant 3.2

@Frequency 1000 Hz
3.2

@Frequency 1000 Hz
ASTM D150-65
Dielectric Strength 200 kV/mm

@Frequency 50.0 Hz,
Temperature 150 °C
5080 kV/in

@Frequency 50.0 Hz,
Temperature 302 °F
ASTM D196-65
280 kV/mm

@Frequency 50.0 Hz,
Temperature 25.0 °C
7110 kV/in

@Frequency 50.0 Hz,
Temperature 77.0 °F
ASTM D196-64
Dielectric Breakdown 4000 - 17500 V
4000 - 17500 V
Minimum; ASTM D149
Descriptive Properties Value Comments
Fire Rating 94-VTM2
UL94 SVT Test Rating