Isoflon PMMA Polymethyl-methacrylate

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Isoflon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PMMA Polymethyl-methacrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Products with good mechanical performances under friction and good dimensional stability, notably in moist environmentsVery rigid, hardHigh machining precisionInformation provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
DIN 53479
Water Absorption 0.30 %
0.30 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength 72.0 MPa
10400 psi
DIN 53455
Elongation at Break 4.0 %
4.0 %
DIN 53455
Tensile Modulus 3.14 GPa
455 ksi
DIN 53457
Thermal Properties Metric English Comments
CTE, linear 68.0 µm/m-°C
37.8 µin/in-°F
DIN 52328
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 210 °C
410 °F
DIN 53736
Maximum Service Temperature, Air 85.0 °C
185 °F
Continuous; DIN 52612
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Continuous; DIN 52612
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+19 ohm-cm
1.00e+19 ohm-cm
DIN 53482
Dielectric Constant 2.9

@Frequency 1000 Hz
2.9

@Frequency 1000 Hz
DIN 53483
Dielectric Strength 20.0 - 30.0 kV/mm
508 - 762 kV/in
DIN 53481
Descriptive Properties Value Comments
Color Transparent
Fire Rating M4
CSTB