Unifrax XPE® NV Substrate Support Mat

Category Ceramic
Manufacturer Unifrax I LLC
Trade Name XPE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax XPE® NV Substrate Support Mat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
XPE® intumescent mat products are designed to function as mechanical support for the ceramic substrate and act as an exhaust gas seal while providing thermal insulation.Unifrax offers a variety of premium and advanced mat products with enhanced performance properties. As a manufacturer of fibers used in a variety of catalytic converter mounting systems, Unifrax has successfully combined fiber making expertise with a state-of-the-art paper manufacturing process to maximize the performance of our catalytic converter support mats. Engineered to meet the performance requirements associated with traditional catalytic converter applications, Unifrax is pleased to offer XPE®-NV substrate support mat.Unifrax XPE-NV provides a unique balance of performance versus value and is recommended for a broad range of catalytic converter substrate support and cone insulation applications. XPE-NV can be engineered to provide excellent thermal stability at inlet gas temperatures up to 950°C. The support mat will expand with increasing relative thickness when first exposed to temperatures in excess of 325°C. Expansion pressure is provided by vermiculite particles trapped in a structural support matrix of Fiberfrax® ceramic fibers. The ceramic fibers also provide resistance to hot gas mat erosion.Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Loss On Ignition >= 6.0 %
>= 6.0 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 0.100 MPa
>= 14.5 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.180 W/m-K

@Temperature 650 °C
1.25 BTU-in/hr-ft²-°F

@Temperature 1200 °F
ASTM C177
Descriptive Properties Value Comments
Binder System (%) 5-9
Fiberfrax® Fibers (%) 30-40
Vermiculite (%) 50-60