Thermal Properties Metric English Comments
CTE, linear 88.7 - 170 µm/m-°C

@Temperature -80.0 - -30.0 °C
49.3 - 94.4 µin/in-°F

@Temperature -112 - -22.0 °F
Average value: 137 µm/m-°C Grade Count:6
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
CTE, linear 50.0 - 170 µm/m-°C
27.8 - 94.4 µin/in-°F
Average value: 102 µm/m-°C Grade Count:13
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 105E3V36327 Acetate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp
Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 307A4000015 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 307A4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 307E0V16310 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 307E4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 360A4000012 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp
Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 360E461312 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp
Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 380A3V32818 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp
Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp
Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp
Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp
Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 485E3720023 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C
61.1 - 94.4 µin/in-°F
ASTM D696
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp
Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl..
CTE, linear 19.8 - 170 µm/m-°C
11.0 - 94.4 µin/in-°F
Average value: 88.1 µm/m-°C Grade Count:36
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
CTE, linear 60.0 - 170 µm/m-°C
33.3 - 94.4 µin/in-°F
Average value: 104 µm/m-°C Grade Count:3
Overview of materials for Nylon, Flexible Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri..
CTE, linear 76.0 - 170 µm/m-°C
42.2 - 94.4 µin/in-°F
Average value: 130 µm/m-°C Grade Count:20
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..
CTE, linear 11.0 - 170 µm/m-°C
6.11 - 94.4 µin/in-°F
Average value: 83.8 µm/m-°C Grade Count:53
Overview of materials for Cellulose Acetate Propionate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val..
CTE, linear 11.0 - 170 µm/m-°C
6.11 - 94.4 µin/in-°F
Average value: 44.8 µm/m-°C Grade Count:36
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Eastman Tenite 360A4861301 Propionate Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Copyright © lookpolymers.com All Rights Reserved