Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lacqrene® 1235 High Impact Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqrene® 1235 High Impact Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACQRENE® 1235 is a high gloss, high impact polystyrene used in injection molding and co-extrusion. This grade produces articles with a surface gloss level equivalent to that of certain grades of ABS.Applications: Toys, Office equipment, White goods, Telephones, Video cassette shutters, Glossy items by coextrusion. Translucent products by blending with 1240.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 5.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ISO 2039-2
Tensile Strength at Break 25.0 MPa
3630 psi
ISO 527-2
Tensile Strength, Yield 31.0 MPa
4500 psi
ISO 527-2
Elongation at Break 30 %
30 %
ISO 527-2
Tensile Modulus 2.05 GPa
297 ksi
ISO 527-2
Flexural Modulus 2.05 GPa
297 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Annealed; ISO 75-2A
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
Unannealed; ISO 75-2A
Vicat Softening Point 89.0 °C
192 °F
50N (T° increase = 5°C/h); ISO 306B50
97.0 °C
207 °F
10N (T° increase = 50°C/h); ISO 306A50
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC93
Dielectric Strength 150 kV/mm
3810 kV/in