Total Lacqrene® 4801  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqrene® 4801  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACQRENE® 4801 is an easy flowing, high impact polystyrene for injection molding. The very good processing characteristics of this grade allows for the production of thin articles with long flow paths or complex shapes. A high level of mechanical properties are retained at very low temperatures (-40°C) which makes this grade particularly suitable for ice cream containers.Applications: Ice cream containers, Models, Presentation boxes, General containers, Medical productsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 200 °C
20 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ISO 2039-2
Tensile Strength at Break 16.0 MPa
2320 psi
ISO 527-2
Tensile Strength, Yield 21.0 MPa
3050 psi
ISO 527-2
Elongation at Break 47 %
47 %
ISO 527-2
Tensile Modulus 1.90 GPa
276 ksi
ISO 527-2
Flexural Modulus 1.90 GPa
276 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
Annealed; ISO 75-2A
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C
156 °F
Unannealed; ISO 75-2A
Vicat Softening Point 76.0 °C
169 °F
50N (T° increase = 5°C/h); ISO 306B50
87.0 °C
189 °F
10N; ISO 306A50
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC93
Dielectric Strength 150 kV/mm
3810 kV/in