Thermal Properties Metric English Comments
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Poco Graphite DFP Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Poco Graphite Glassmate® GM Graphite
This material has high strength and durability for applications with high wear. An exceptional insert material for precision thread pick up and long production runs.
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Poco Graphite SFG Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Poco Graphite ZXF-5Q Industrial Grade Graphite
SSH hardness is 86.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p..
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Poco Graphite DFP-3-2 Ion Implant Grade Graphite
This is a high strength graphite that has reduced porosity. DFP-3-2 has long been the standard for components that exhibit long life and reduced erosion rates.
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Poco Graphite HPD Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder
A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder
Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder ..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder
A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder
Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder
Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 - 400 °C
4.50 µin/in-°F

@Temperature 68.0 - 752 °F
DIN EN 821-1
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications.
CTE, linear 8.10 µm/m-°C

@Temperature 25.0 - 1000 °C
4.50 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek AD-90 Alumina (nom. 90% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Cotronics Resbond™ 907 High Temperature Ceramic Adhesive, Industrial Strength
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Cotronics Resbond™ 908 High Temperature Ceramic Adhesive, Moisture Proof
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Cotronics Resbond™ 940 High Temperature Ceramic Adhesive, Fast Set
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Cotronics Resbond™ 989 High Temperature, High Purity Alumina Adhesive, General Purpose
CTE, linear 8.10 µm/m-°C

@Temperature 25.0 - 1000 °C
4.50 µin/in-°F

@Temperature 77.0 - 1830 °F
Astro Met ZTA 96 Zirconia Toughened Alumina
General Description:ZTA-96 is a zirconia toughened alumina ceramic that exhibits excellent wear and corrosion resistance along with high strength and toughness. Astro Met has developed ZTA-96 zircon..
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Poco Graphite Glassmate® HT Graphite
This high strength material has an oxidation inhibitor that raises the oxidation threshold. Service temperature can be raised to 600°C; graphites are subject to oxidation above 450°C
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.