Cotronics Resbond™ 940 High Temperature Ceramic Adhesive, Fast Set

Category Ceramic
Manufacturer Cotronics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Resbond™ 940 High Temperature Ceramic Adhesive, Fast Set.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mechanical Properties Metric English Comments
Flexural Strength 3.45 MPa
500 psi
Compressive Strength 27.6 MPa
4000 psi
Thermal Properties Metric English Comments
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 °C
4.50 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.15 W/m-K
8.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1090 °C
2000 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Dielectric Strength 4.92 kV/mm
125 kV/in