Poco Graphite Glassmate® HT Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name Glassmate®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite Glassmate® HT Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This high strength material has an oxidation inhibitor that raises the oxidation threshold. Service temperature can be raised to 600°C; graphites are subject to oxidation above 450°C
Physical Properties Metric English Comments
Apparent Bulk Density 1.74 g/cc
0.0629 lb/in³
Particle Size 5.0 µm
5.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
Flexural Strength 81.0 MPa
11700 psi
Compressive Strength 136 MPa
19700 psi
Thermal Properties Metric English Comments
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Thermal Conductivity 85.0 W/m-K
590 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00147 ohm-cm
0.00147 ohm-cm
Descriptive Properties Value Comments
Oxidation Threshold 607°C