CTE, linear 64.8 - 81.0 µm/m-°C
36.0 - 45.0 µin/in-°F
Average value: 71.6 µm/m-°C Grade Count:5
Overview of materials for Nylon 66, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri..
CTE, linear 64.8 µm/m-°C

@Temperature -40.0 - 82.2 °C
36.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 4800-10 Polycarbonate
EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca..
CTE, linear 64.8 µm/m-°C

@Temperature -40.0 - 82.2 °C
36.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 4850-10 Polycarbonate
EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr..
CTE, linear 64.8 µm/m-°C

@Temperature -40.0 - 82.2 °C
36.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 4850-19 Polycarbonate
EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Styron EMERGEâ„¢ 8600-10 Polycarbonate
EMERGEâ„¢ PC 8600-10 is a translucent, ignition-resistant polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental ..
CTE, linear 64.8 µm/m-°C

@Temperature -40.0 - 82.2 °C
36.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 893-10 Polycarbonate
CALIBREâ„¢ 893-10 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo..
CTE, linear 64.8 µm/m-°C

@Temperature -40.0 - 82.2 °C
36.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 893-20 Polycarbonate
CALIBREâ„¢ 893-20 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo..
CTE, linear 64.8 µm/m-°C

@Temperature -40.0 - 82.2 °C
36.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 4800-19 Polycarbonate
EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca..
CTE, linear 64.8 µm/m-°C

@Temperature -40.0 - 82.2 °C
36.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 4800-7 Polycarbonate
EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar..
CTE, linear 64.8 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D-3386
CMT Materials REN Shape® 450 Prototype Tool & Modeling Board
REN Shape 450 is the preferred modeling board for pattern makers throughout the world. The outstanding dimensional stability and its ability to hold precise tolerances even after exposure to heat h..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 7450 Rigid PVC, Extrusion
Georgia Gulf 7450 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: Excellent ToughnessSatin Surface AppearanceColorabilityChemical Res..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 7456 Rigid PVC, Extrusion
Georgia Gulf 7456 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessWeatherabilityWeldabilityChemical ResistanceEase of Proces..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 5055 Rigid PVC, Extrusion, White
Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 7055 Rigid PVC, Extrusion
Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 7555 Rigid PVC, Extrusion, Natural
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 7555 Rigid PVC, Extrusion, White
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 7765 Rigid PVC, Extrusion
Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zo..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 7768 Rigid PVC, Extrusion
Georgia Gulf 7768 is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermofil P-9900-0576 Unreinforced, Flame Retardant, Heat Stabilized
Information provided by Asahi Thermofil
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 5006 Rigid PVC, Extrusion, Natural
Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 5006 Rigid PVC, Extrusion, White
Georgia Gulf 5006 White is a rigid PVC pellet compound designed for extrusion of rigid PVC house siding, window profiles and various contours where maximum weather resistance is required. Georgia G..
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 5055 Rigid PVC, Extrusion, Natural
Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p..