Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 64.8 - 81.0 µm/m-°C | 36.0 - 45.0 µin/in-°F | Average value: 71.6 µm/m-°C Grade Count:5 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
CTE, linear | 8.00 - 81.0 µm/m-°C | 4.44 - 45.0 µin/in-°F | Average value: 52.4 µm/m-°C Grade Count:18 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |