Axiall 5006 Rigid PVC, Extrusion, Natural

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 5006 Rigid PVC, Extrusion, Natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf 5006 is widely used for high gloss custom profile, sheet applications. USDA approval allows for use in walk-in coolers and refrigerated trucks. Single or twin screw machines may be used to convert Georgia Gulf 5006. It has been designed with good impact at ambient temperatures. The high flexural and tensile strength make it highly suitable for structural installation. The extrusion flow characteristics are excellent in complicated profiles. It is easily colored using concentrates. Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D-785
Hardness, Shore D 82
82
ASTM D-2240
Tensile Strength, Yield 49.0 MPa
7100 psi
ASTM D-638
Tensile Modulus 3.10 GPa
450 ksi
ASTM D-638
Flexural Strength 84.1 MPa
12200 psi
ASTM D-790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D-790
Izod Impact, Notched 0.801 J/cm

@Thickness 6.35 mm
1.50 ft-lb/in

@Thickness 0.250 in
ASTM D-256
1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 137 kJ/m²
65.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
156 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F
Descriptive Properties Value Comments
Cell Classification 13464
ASTM D-1784