Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer Ensinger
Trade Name Hydel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machining (unlike conventional carbon fibers), consistent electrical properties, excellent surface quality and minimal sloughing. It also possesses outstanding toughness and excellent thermal stability.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Water Absorption 0.25 %

@Temperature 22.8 °C,
Time 86400 sec
0.25 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.8 MPa
9400 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Strength 112 MPa
16200 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Compressive Strength 112 MPa
16200 psi
ASTM D695
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 52.2 µm/m-°C
29.0 µin/in-°F
Maximum Service Temperature, Air 171 °C
340 °F
continuous
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+6 - 1.00e+9 ohm
1.00e+6 - 1.00e+9 ohm
ASTM D257
Descriptive Properties Value Comments
Base Material Polycarbonate