Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 22.0 - 47.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 - 26.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Lexan® LC120 PC (Asia Pacific) |
|||
CTE, linear | 24.0 - 47.0 µm/m-°C | 13.3 - 26.1 µin/in-°F | Average value: 33.4 µm/m-°C Grade Count:5 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear | 14.0 - 47.0 µm/m-°C | 7.78 - 26.1 µin/in-°F | Average value: 23.4 µm/m-°C Grade Count:5 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
CTE, linear | 3.60 - 47.0 µm/m-°C | 2.00 - 26.1 µin/in-°F | Average value: 24.7 µm/m-°C Grade Count:19 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |