Polymer Property : CTE, linear = 148 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 148 µm/m-°C

@Temperature 20.0 °C
82.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech CastAlloy Weatherable Sheet
Description: Weatherable SheetInformation provided by Spartech.
CTE, linear 148 µm/m-°C
82.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy
Product Description: EPO-TEK® 305 is a two component, semi-rigid, optical grade epoxy for semiconductor packaging of fiber optics, optoelectronics and medical devices. It is an electrically and th..
CTE, linear 148 µm/m-°C
82.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® E3037 Epoxy
Material Description: A single component, electrically conductive, thixotropic silver-filled epoxy for die-attach and SMD-attach inside hybrid microelectronics.Information Provided by Epoxy Technolo..
CTE, linear 148 µm/m-°C
82.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® H31LV Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H31LV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electron..
CTE, linear 148 µm/m-°C
82.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® H37-MP Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H37-MP is a single component, electrically conductive, thixotropic silver-filled adhesive for die-attach and SMD attach inside hybrid microelectronic packages. Also av..