Description: Weatherable SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 47.2 MPa
6850 psi
ASTM D638
Tensile Modulus 2.34 GPa
339 ksi
ASTM D638
Flexural Yield Strength 71.0 MPa
10300 psi
ASTM D790
Flexural Modulus 2.48 GPa
359 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 148 µm/m-°C

@Temperature 20.0 °C
82.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 89.4 °C
193 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523