Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 148 µm/m-°C @Temperature 20.0 °C |
82.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech CastAlloy Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |