Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 110 - 200 µm/m-°C @Temperature 20.0 °C |
61.1 - 111 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Rotuba 855, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
CTE, linear | 110 - 200 µm/m-°C @Temperature 20.0 °C |
61.1 - 111 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Rotuba 856, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
CTE, linear | 150 - 200 µm/m-°C @Temperature 20.0 - 80.0 °C |
83.3 - 111 µin/in-°F @Temperature 68.0 - 176 °F |
DIN 53 752-A |
Orbilan ORBILAN® PE 1000 UHMW-PE Orbilan PE 1000 plastics distinguish themselves through their optimal balance of the technical features with regard to wear-resistance and impact resistance. The areas of use range from general mac.. |
|||
CTE, linear | 20.0 - 200 µm/m-°C | 11.1 - 111 µin/in-°F | Average value: 191 µm/m-°C Grade Count:110 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
CTE, linear | 120 - 200 µm/m-°C | 66.7 - 111 µin/in-°F | 25°C to 100°C; ASTM D696 |
Guarniflon MFA Fluoropolymer It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It .. |
|||
CTE, linear | 120 - 200 µm/m-°C | 66.7 - 111 µin/in-°F | 25°C to 100°C; ASTM D696 |
Guarniflon PFA Perfluoroalkoxy Polymer Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli.. |
|||
CTE, linear | 150 - 200 µm/m-°C @Temperature 20.0 - 80.0 °C |
83.3 - 111 µin/in-°F @Temperature 68.0 - 176 °F |
DIN 53 752-A |
Orbilan ORBILAN® PE 500 HMW-PE Orbilan PE 500 plastic is used as cutting boards for the food industry and gastronomy, in refrigeration chambers as ram protection and for swing doors as well as at sports grounds for sheets or hand.. |
|||
CTE, linear | 120 - 200 µm/m-°C | 66.7 - 111 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)
(discontinued **) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
CTE, linear | 120 - 200 µm/m-°C | 66.7 - 111 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
CTE, linear | 34.2 - 200 µm/m-°C | 19.0 - 111 µin/in-°F | Average value: 123 µm/m-°C Grade Count:11 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
CTE, linear | 187 - 200 µm/m-°C | 104 - 111 µin/in-°F | Average value: 192 µm/m-°C Grade Count:5 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |