Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 155 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 40.6 - 155 °C
105 - 311 °F
Average value: 68.4 °C Grade Count:152
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Deflection Temperature at 1.8 MPa (264 psi) 46.0 - 155 °C
115 - 311 °F
Average value: 117 °C Grade Count:92
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
Deflection Temperature at 1.8 MPa (264 psi) 35.6 - 155 °C
96.0 - 311 °F
Average value: 122 °C Grade Count:93
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..