Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 35.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 35.6 °C
96.0 °F
ASTM D648
RheTech Products E206-01 Linear Low Density Polyethylene, Black
Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 35.6 °C
96.0 °F
Aclo Accutech Polypropylene Homopolymer HP0339G5M25CL Glass/Mineral Reinforced Coupled
Deflection Temperature at 1.8 MPa (264 psi) 35.6 - 155 °C
96.0 - 311 °F
Average value: 122 °C Grade Count:93
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..