Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 35.6 °C | 96.0 °F | ASTM D648 |
RheTech Products E206-01 Linear Low Density Polyethylene, Black Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 35.6 °C | 96.0 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339G5M25CL Glass/Mineral Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 35.6 - 155 °C | 96.0 - 311 °F | Average value: 122 °C Grade Count:93 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |