Borealis Daploy™ WB260HMS Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name Daploy™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Daploy™ WB260HMS Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Daploy™ WB260HMS is a propylene-based, structurally isomeric polymer. Applications: cushioning and protective packaging, door liners, lightweight packaging trays, beakers and containers, microwaveable food packaging, parcel shelves, technical foams for automotive applications such as headliners, carpet backing, thermoformable foamed films and sheets, under the hood acoustic panels, water shields, and thermal and acoustic insulation.Information provided by Borealis AG
Physical Properties Metric English Comments
Melt Flow 2.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ISO 527-2
Elongation at Yield 13 %
13 %
ISO 527-2
Tensile Modulus 0.900 GPa
131 ksi
ISO 527-2
Flexural Modulus 0.850 GPa
123 ksi
ISO 178
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
ISO 75-2