Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PETROTHENE GA574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items.Regulatory Status: GA574189 meets the requirements of the Food and Drug Administration regulation, 21 CFR 1 77.1 520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food..." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing GA574189 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D1505
Melt Flow 50 g/10 min
50 g/10 min
ASTM D1238
Spiral Flow 49.0 cm
19.3 in
Equistar test
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength at Break 10.3 MPa
1500 psi
ASTM D638
Tensile Strength, Yield 14.5 MPa
2100 psi
20"/min; ASTM D638
Elongation at Yield 8.2 %
8.2 %
20"/min; ASTM D638
1% Secant Modulus 441 MPa
64000 psi
0.5"/min; ASTM D790
2% Secant Modulus 0.414 GPa
60.0 ksi
0.5"/min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ASTM D648
Vicat Softening Point 96.0 °C
205 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<SUB>50</SUB>; ASTM D746
Processing Properties Metric English Comments
Rear Barrel Temperature 177 °C
350 °F
Middle Barrel Temperature 191 °C
375 °F
Front Barrel Temperature 204 °C
400 °F
Nozzle Temperature 204 °C
400 °F
Copyright © lookpolymers.com All Rights Reserved