Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 172 °C

@Thickness 3.18 mm
342 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Nymax™ 600 A Zip 22 Natural Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
120°C/h; ISO 75/1
Polykemi AB POLYshine PBT D223 Q30 FR PBT, Mineral Reinforced, Flame Retardant
Information provided by Polykemi AB
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
ASTM D648
Asahi Kasei Tenac® 2013A Acetal Homopolymer, UV Stabilized  (discontinued **)
Similar to 3013A, but higher in molecular weight.Applications: Pipe fittings, rollers, exterior automotive parts.This product is not a part of the standard product line dated 2003.
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
ASTM D648
Asahi Kasei Tenac® 5012 Acetal Homopolymer  (discontinued **)
Standard-flow grade, with reduced stiffness and increased elongation through addition of special polymers.Applications: Clips, fasteners, press-fit parts.This product is not a part of the standard p..
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
ASTM D648
Asahi Kasei Tenac® GT525 Acetal Homopolymer, 25% Glass Beads  (discontinued **)
25% glass beads-filled grade with superior isotropic dimensional stability.Applications: Speedometer frames.This product is not a part of the standard product line dated 2003.
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
ASTM D648
Asahi Kasei Tenac® LT805 Acetal Homopolymer, Low Friction Grade  (discontinued **)
Excellent friction and wear on metals.Applications: Keyboard parts, bearings for office machines, gears.This product is not a part of the standard product line dated 2003.
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
Covestro Apec® DP 1-9359/7 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer M..
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
ISO 75-1,-2
Lanxess Durethan® BC 30 S 000000 Nylon 6
PA 6, non-reinforced, injection moldingInformation provided by LANXESS.
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12
LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated.
Deflection Temperature at 0.46 MPa (66 psi) 172 °C

@Thickness 3.20 mm
342 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI
LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 172 °C

@Thickness 6.40 mm
342 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL GTX GTX905 PPE+PS+PA
Automotive.
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
ISO 75-1/-2
Covestro Apec® 1897 Polycarbonate
Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=182 °CPreprocessingMax. Water content
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
ASTM D648
A. Schulman ComAlloy Hiloy® 662 Nylon 6, Glass Bead Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Glass Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
Covestro Apec® 1805 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation pr..
Deflection Temperature at 0.46 MPa (66 psi) 172 °C

@Thickness 3.20 mm
342 °F

@Thickness 0.126 in
ASTM D648
Covestro Apec® DP9-9353 High-Heat Polycarbonate, UV Stabilized  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..