A. Schulman ComAlloy Hiloy® 662 Nylon 6, Glass Bead Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Bead Filled
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 662 Nylon 6, Glass Bead Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.20% Glass Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Ultimate 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 205 - 225 °C
401 - 437 °F
Deflection Temperature at 0.46 MPa (66 psi) 172 °C
342 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 260 - 271 °C
500 - 520 °F