Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 120 - 130 °C | 248 - 266 °F | ASTM D1525, HDT Method B |
Loxim 820 01 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 120 - 130 °C | 248 - 266 °F | ASTM D1525, HDT Method B |
Loxim 820 12 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 113 - 130 °C | 235 - 266 °F | Average value: 120 °C Grade Count:3 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 - 130 °C | 169 - 266 °F | Average value: 107 °C Grade Count:36 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |