Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 820 01 HB Polypropylene Compound, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 820 01 HB Polypropylene Compound, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Filler Content 20 %
20 %
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 - 45.0 MPa
5800 - 6530 psi
ASTM D683
Elongation at Break 8.0 - 12 %
8.0 - 12 %
ASTM D638
Flexural Modulus 3.00 - 3.50 GPa
435 - 508 ksi
ASTM D790
Izod Impact, Notched 0.400 - 0.600 J/cm
0.749 - 1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 - 130 °C
248 - 266 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in