Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | ASTM D648 |
Ineos R01C-01 Polypropylene Random Copolymer This is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding. Applications that require good see-through clarity combined with good heat resistance .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | Unannealed; ASTM D648 |
Multibase Multi-Flamâ„¢ 205 HFRI Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | unannealed (0.250 in); ASTM D648 |
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | ISO 75-2/B |
ExxonMobil Exxtral™ CNK 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa &.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | ISO 75-2/B |
ExxonMobil PP7033L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin characterized with low flow. It is suitable for extrusion applications like sheet and thermoforming. It is also suitable for molding applications like.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | ASTM D648 |
ExxonMobil PP9574E6 Polypropylene Homopolymer Product Description: A highly clarified random copolymer resin designed for general purpose injection molding applications requiring resistance to build up of static electricity.Availability: North.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | ASTM D648 |
Clariant Remafin PP1100NAT Polypropylene Impact Modified Copolymer Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow UNIVAL™ DMDH-6400 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDH-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, water and fruit drinks. In a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | ASTM D648 |
Aclo Accucomp Polypropylene CPO406L Copolymer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 - 130 °C | 169 - 266 °F | Average value: 107 °C Grade Count:36 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |