Polyram RamLloy PJ701 ABS/ASA, General Purpose

Category Polymer , Thermoplastic , ABS Polymer , ASA Polymer
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamLloy PJ701 ABS/ASA, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PJ 701 IS A GENERAL PURPOSE INJECTION MOLDING ASA& ABS ALLOY . IT HAS GOOD MECHANICAL PROPERTIES SIMILAR TO ABS AND MUCH BETTER WEATHER RESISTANCE. AN IDEAL ECONOMIC CHOICE.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Melt Flow 15 g/10 min

@Load 2.10 kg,
Temperature 220 °C
15 g/10 min

@Load 4.63 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM-D638
Elongation at Break 90 %
90 %
ASTM-D638
Tensile Modulus 1.80 GPa
261 ksi
ASTM-D790
Flexural Strength 65.0 MPa
9430 psi
ASTM-D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM-D790
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Hot Ball Pressure Test 90.0 °C
194 °F
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
DIN 53461
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
DIN 53482