Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
ASTM D648
Polymer Resources NY6/12-GP1 General Purpose Nylon 612
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP FARADEX PS003E PA 6
LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Europe-Africa-Middle East)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Annealed, 0.125 in bars; ASTM D648
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated  (discontinued **)
Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Deflection Temperature at 0.46 MPa (66 psi) 171 - 179 °C
340 - 355 °F
Average value: 177 °C Grade Count:5
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ..
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed; ASTM D648
Techmer ES Elastoblend® PA6 IM 7040 MB
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro..
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed; ASTM D648
Techmer ES Elastoblend® PA6 IM 7050
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro..
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI
LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6 TSX10 Nylon 6
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6 TSX15 Nylon 6
Availability: North AmericaForms: PelletsAdditive: PTFE+ Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® PA6 NAT001 Nylon 6
Availability: North AmericaForms: PelletsFeatures: Good Processability and High FlowAppearance: NaturalTPCI# 1327102Information provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
ASTM Test
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry)
Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven..
Deflection Temperature at 0.46 MPa (66 psi) 171 °C

@Thickness 3.20 mm
340 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP
LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
method Bf; ISO 75-2
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
ISO 75-1/-2
DuPont Performance Polymers Delrin® 588P NC010 Acetal (POM)
Nucleated Medium Viscosity Acetal HomopolymerInformation provided by DuPont Performance Polymers
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
ASTM D648
Clariant Renol 6253 Nylon 6, High Impact
Data provided by Clariant Masterbatches
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
ASTM D648
Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized
Data provided by Clariant Masterbatches
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
ASTM D648
Adell BD-10 Nylon 6, Ultra High Impact
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
ASTM D648
Adell BD-30 Nylon 6, Ultra High Impact
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
ASTM D648
Ashley Polymers Ashlene® RH190-PF Acetal, PTFE Filled
A wear-resistant grade homopolymer resin with 1.5% PTFE.Data provided by the manufacturer
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N2200 HL Nylon 6/6  (discontinued **)
Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackProcessing Method: Injection MoldingInformation pr..
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed, 0.125 in bars; ASTM D648
PolyOne Edgetek® ATH-25GF/000 Acetal-Homopolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed, 0.125 in bars; ASTM D648
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.