Material Notes:
A wear-resistant grade homopolymer resin with 1.5% PTFE.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.19 %
0.19 %
ASTM D570
Moisture Absorption at Equilibrium 0.20 %
0.20 %
50% RH; ASTM D570
Melt Flow 6.0 g/10 min
6.0 g/10 min
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 69.0 MPa
10000 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0060

@Frequency 1000 Hz
0.0060

@Frequency 1000 Hz
ASTM D150