Ravago Manufacturing Americas Hylon® N2200 HL Nylon 6/6  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N2200 HL Nylon 6/6  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackProcessing Method: Injection MoldingInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Water Absorption 1.6 %

@Time 86400 sec
1.6 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 119
119
ASTM D785
Tensile Strength at Break 72.4 MPa
10500 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Unannealed; ASTM D648