Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648-95 |
Multibase Multi-Pro® 0505 RC Black 5.2% Glass Filled Polypropylene This product was specially designed for one customer's glass filled polypropylene application.Data provided by Multibase. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648 |
RheTech Products E204-01 High Density Polyethylene, Black Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
Polymer Industries Polyslick UHMW Rod Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
Polymer Industries Polyslick UHMW Profile Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | 120°C/h; ASTM D648 |
Total Finaclear® 520 Clear Impact Polystyrene
(discontinued **) Finaclear® 520 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles. Complemented by inherent repr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | 120°C/h; ASTM D648 |
Total Finaclear® 521 Clear Impact Polystyrene
(discontinued **) Finaclear® 521 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with othe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 72.8 °C | 149 - 163 °F | Average value: 68.7 °C Grade Count:5 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 95.0 °C | 149 - 203 °F | Average value: 71.2 °C Grade Count:14 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | HDT/A; ASTM D648 |
GEHR Plastics ECOGEHR® PA 6.10 Nylon 6.10 Dry, 60% Sebacic Acid Nylon 6.10 is 60 % sebacic acid, which is obtained from castor oil. This material combines a low density (for polyamide) with good cold impact strength, and its low water absorption makes it very di.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75 |
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648-82 |
Micropol Microcene MC121 Metallocene Based Polyethylene Rotational Molding Powder Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648 |
Borealis Borecene™ RM8342 Linear Polyethylene for Rotational Molding Borecene RM8342 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648 |
Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding Borecene RM8342RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8342RC is a special grade, which has passed many rigorous tests and can be cons.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
DSM Arnitel® PB420 TPC-ET Blow Molding Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
DSM Arnitel® PB420-B TPC-ET Blow Molding Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
DSM Arnitel® PL461 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
DSM Arnitel® PM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 70.0 °C | 149 - 158 °F | ASTM D648-98c |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 70.0 °C | 149 - 158 °F | ASTM D648-98c |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 66.0 °C | 149 - 151 °F | ASTM D648 |
3D Systems Accura® Bluestone™ Plastic for SLA® Systems A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 70.0 °C | 149 - 158 °F | |
C.O.I.M. EXTER S® S 108 A Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 108 A: Resin for van.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648 |
RheTech Products E204-00 High Density Polyethylene, Natural Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 202 °C | 149 - 396 °F | Average value: 142 °C Grade Count:80 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |